Axel REE Tests Simpler Rare Earth Processing at Woolrich

Axel REE’s Woolrich carbonate test bypassed a dedicated impurity-removal stage, but field testing must establish whether the process can scale up.

Wade Turner 3 min read
lab, analysis, diagnostics, hospital, test tube, test, tests, medical, the doctor, test tubes, medic, treatment, patient, dia

Axel REE produced its first mixed rare earth carbonate from Woolrich leach solutions with 54.41% total rare earth oxides, without a dedicated impurity-removal stage in the laboratory test circuit.

Axel REE (ASX: AXL) has produced its first mixed rare earth carbonate from its Woolrich deposit in Brazil, demonstrating a processing step that could simplify its proposed production route. The laboratory circuit produced material containing 54.41% total rare earth oxides without a dedicated stage to remove impurities.

The result connects earlier column-leaching work with production of a carbonate intermediate. It does not yet establish commercial viability: the next challenge is to reproduce the performance using representative solutions from controlled field testing.

A treatment stage left out of the laboratory circuit

Testing at CORE Resources in Australia combined magnesium sulphate column leaching with magnesium bicarbonate precipitation, which brings dissolved rare earths out of solution. The MREC04 circuit produced 15.11 grams of dried carbonate from a blend of column-test solutions and filtrate from an earlier precipitation test, according to Stockhead Resources.

Precipitation efficiencies reached 97% for total rare earth oxides and 99% for magnet rare earth oxides. Those figures measure the precipitation step, rather than overall recovery from the mineralized deposit through to a finished product.

Low aluminum and iron concentrations in the feed supported precipitation without a separate impurity-removal stage. Conventional carbonate processing can require that treatment before precipitation, adding equipment and operating costs. Avoiding it could therefore simplify Woolrich’s processing route, provided the result holds under representative operating conditions.

Low aluminum and iron concentrations in the feed supported precipitation without a separate impurity-removal stage.

The carbonate also contained uranium at 0.78 parts per million and thorium at 0.10 parts per million. Managing director Dr Patience Mpofu identified those low concentrations as a potential benefit of Woolrich’s naturally buffered mineralized regolith.

Magnet oxides drive the indicative product value

Magnet rare earth oxides represented 35.9% of the product’s total rare earth oxide content. That included 34.1% neodymium-praseodymium and 1.75% dysprosium-terbium.

Using rare earth oxide spot prices from October 21, 2026, Axel calculated an indicative gross contained oxide basket value of US$42.72 per kilogram of total rare earth oxides. Neodymium-praseodymium and dysprosium-terbium contributed about 92.8% of that calculated value, concentrating the product’s indicative worth in its magnet materials.

That basket value is not a realized selling price for the mixed carbonate. It values the contained oxides and should not be treated as revenue or a measure of project profitability.

Field tests must connect chemistry with engineering

Woolrich contains a resource of 264.6 million tonnes at around 1,100 parts per million total rare earth oxides. It forms part of the broader Caladão resource of 708.6 million tonnes at 1,443 parts per million.

Axel is progressing technical design and preparatory studies for a controlled field test at Woolrich, including hydrogeological, geotechnical and environmental assessments. The field work is intended to assess rare earth recovery and solution chemistry under controlled in-situ conditions.

Further metallurgical work will examine precipitation conditions, reagent consumption, product washing and impurity control. Subsequent processing tests will assess whether the laboratory performance can be repeated with representative solutions. Together, those results will inform the proposed in-situ recovery process and future engineering and economic studies—the work needed to determine whether omitting a treatment stage delivers a practical commercial benefit.

Key facts

  • Company: Axel REE (ASX: AXL); Woolrich deposit, Brazil
  • Carbonate grade: 54.41% total rare earth oxides; magnet oxides represented 35.9% of TREO
  • Precipitation efficiency: 97% for total rare earth oxides and 99% for magnet rare earth oxides
  • Processing milestone: 15.11 grams of dried carbonate produced without a dedicated impurity-removal stage

Sources